Aha ngwaahịa | Plastic bọọlụ igel | |||
Ihe onwunwe | PP, PE, PVC, CPVC, PVDF, wdg | |||
Ogo mm | Ebe dị n'elu m2/m3 | Olu efu% | Njupụta njupụta Kg/m3 | Factorm mbukota akọrọ-1 |
40 | 300 | 87 | 102 | 473 |
Enwere ike ịme nkwakọ ngwaahịa ụlọ elu site na plastik na-eguzogide okpomọkụ na kemịkalụ corrosion, gụnyere polyethylene (PE), polypropylene (PP), polypropylene siri ike (RPP), polyvinyl chloride (PVC), chlorinated polyvinyl chloride (CPVC), polyvinyiidene fluoride (PVDF) na Polytetrafluoroethylene (PTFE). Okpomọkụ dị na mgbasa ozi sitere na 60 Celsius C ruo 280 Celsius C.
Arụmọrụ/Ihe | PE | PP | RPP | PVC | CPVC | PVDF |
Njupụta (g/cm3) (mgbe akpụzichara ntụtụ) | 0.98 | 0.96 | 1.2 | 1.7 | 1.8 | 1.8 |
Okpomọkụ ọrụ (℃) | 90 | >100 | >120 | >60 | >90 | >150 |
Chemical corrosion eguzogide | ỌMA | ỌMA | ỌMA | ỌMA | ỌMA | ỌMA |
Ike mkpakọ (Mpa) | >6.0 | >6.0 | >6.0 | >6.0 | >6.0 | >6.0 |
Arụmọrụ/Ihe | PE | PP | RPP | PVC | CPVC | PVDF |
Njupụta (g/cm3) (mgbe akpụzichara ntụtụ) | 0.98 | 0.96 | 1.2 | 1.7 | 1.8 | 1.8 |
Okpomọkụ ọrụ (℃) | 90 | >100 | >120 | >60 | >90 | >150 |
Chemical corrosion eguzogide | ỌMA | ỌMA | ỌMA | ỌMA | ỌMA | ỌMA |
Ike mkpakọ (Mpa) | >6.0 | >6.0 | >6.0 | >6.0 | >6.0 | >6.0 |